TWISTED YARN

USER INDUSTRIES - TEXTILES: Embroidery, Weaving, Warping. KNITTING: Knits, Braids, Sweaters & Knitwears. CORDS & ROPES, LINGERIE.

Twisted yarn

MH type: Supported yarn made by wrapping filament yarn around metallic yarn in required twist to give support and shine.

MX type: Supported yarn made by using two mono filament yarns wrapped around metallic yarn to give strength & shiny effect

ST Type: Supported or Rounded yarn made by wrapping metallica yarn around filament in required twist to give a glamourous effect

Specifications

Mixing Filaments Denier of Filament
Polyester 50, 75, 100, 150, 300, 450
Viscose / Rayon 75, 150
Nylon 20, 40, 70
Cotton 300, 600
Special Filaments and Denier available with various twists














Technical Specifications

12 micron (G- 50) Metallic yarn, made from Metallised Lacquer coated Polyester film, is twisted with filament yarn to increase the strength & improve the look of the yarn.

Met + Filament Yarn Type Length/ kg Denier
1/69” + 20D Nylon MX Silver approx 88,000 m
Color approx 84,000 m
104 D
109 D
1/71” + 75D Poly ST Silver approx 55,000 m
Color approx 53,000 m
150 D
155 D
1/69” + 150D Viscose ST Silver approx 39,000 m
Color approx 37,000 m
237 D
240 D
1/110” + 75D Nylon MH Silver approx 80,000 m
Color approx 78,000 m
113 D
115 D

* We have the capacity & capability to manufacture twisted yarns of any size specified by the customer to meet their specific requirements




CHEMICAL CHARACTERISTICS FOR TWISTED YARN

CHEMICAL CHARACTERISTICS FOR TWISTED YARN
Fastness to Light 15 hrs (Fadeometer)
Fastness to Crocking Min 3
Fastness to Laundering
Acetone 100% 21°C 30 min
Benzene ” ” ”
Ethyl Alcohol ” ” ”
Carbon disulfide ” ” ”
Carbon tetrachloride ” ” ”
Tri choloro ethylene ” ” ”
Boiling 60°C 20 min
Oxalic Acid 2% 60°C 10 min
Monogen 0.2% 60°C 20 min
Dry Heat On cloth (wet) 130°C 30 sec.

Users of our yarns are recommended to conduct required tests prior to process of bulk quantities of their products incorporating our yarns in their best interests.

We believe this information to be reliable and the best currently available on the subject. Revisions will be made as additional information and experience are obtained. Venlon makes no guarantee of results and assumes no obligation or liability whatsoever in connection with this publication.



TEST REPORT FOR TWISTED YARN


Product: 12 mic M Yarn + 150 D Viscose

Description Standard Value
Total Yarn Count/ Denier 247
Elongation 23 – 25%
Tenacity 25 – 28
Direction S / Z
TPM range 1100 – 1300
Color Fastness – Rubbing 4-5
Color Fastness – Laundering 30°C, 30 min., Detergent 4g/ltr 4-5
Color Fastnes – Light 50°C, Humidity 40% > 4
Acetone/ Benzene/ Ethyl Alcohol 100%, 21°C, 30 minutes
Boiling 60°C, 20 minutes
Dry Heat on wet cloth 130°C, 30 seconds


TEST REPORT FOR TWISTED YARN

Product: 12 mc M Yarn + 80 D Polyester

Description Standard Value
Total Yarn Count/ Denier 150
Elongation 23 – 25%
Tenacity 25 – 28
Direction S / Z
TPM range 1300 – 1500
Color Fastness – Rubbing 4-5
Color Fastness – Laundering 30°C, 30 min., Detergent 4g/ltr 4-5
Color Fastnes – Light 50°C, Humidity 40% > 4
Acetone/ Benzene/ Ethyl Alcohol 100%, 21°C, 30 minutes
Boiling 60°C, 20 minutes
Dry Heat on wet cloth 130°C, 30 seconds




TEST REPORT FOR TWISTED YARN


Product: 12 mic M Yarn + 20 D Viscose

Description Standard Value
Total Yarn Count/ Denier 104
Elongation 23 – 25%
Tenacity 25 – 28
Direction S / Z
TPM range 250 – 450
Color Fastness – Rubbing 4-5
Color Fastness – Laundering 30°C, 30 min., Detergent 4g/ltr 4-5
Color Fastnes – Light 50°C, Humidity 40% > 4
Acetone/ Benzene/ Ethyl Alcohol 100%, 21°C, 30 minutes
Boiling 60°C, 20 minutes
Dry Heat on wet cloth 130°C, 30 seconds